LINQCELL NWM 250 | 0.25mm Nickel Wire Mesh

Harmonization Code : 7508.10.00.00 | Cloth, grill and netting, of nickel wire

LINQCELL NWM250 | 0.25mm Nickel Wire Mesh roll

Main features

  • 0.25 mm wire diameter
  • Excellent chemical stability and anti-corrosion resistance
  • High electrical conductivity

Product Description

LINQCELL NWM250 is a finely woven wire mesh made from high-purity nickel alloy, with a wire diameter of 0.25 mm and a nickel content of at least 99.9%. Its mesh size and uniformity complies with GB/T 17492. This mesh offers excellent electrical conductivity, chemical stability, corrosion resistance, and mechanical durability. Its versatile properties make NWM250 suitable for different electrochemical devices, including water electrolyzers, fuel cells, and batteries, such as nickel–metal hydride (NiMH) and nickel–cadmium (NiCd) batteries.

Key Features:

  • High corrosion resistance
  • Very low impurities
  • Cheaper and more cost efficient than sintered titanium

In water electrolyzers and fuel cells, LINQCELL NWM250 can be used both as a gas diffusion layer, facilitating mass and electron transfer within the device, and gas diffusion electrode when catalyst layers are directly applied to it. Its suitability for alkaline systems has established it as a standard electrode material in alkaline water electrolyzers.

Highly Recommended for:

LINQCELL NWM250 comes in different mesh counts (30, 40, 46, and 60, allowing precise tuning of diffusivity to meet various device design requirements. It is also available in two Ni grades: N4 (Ni201), and N6 (Ni200).

Product Family

NWM250/185X185N6M40

1855 x 1855 mm Sheet - N6 Alloy
1. Select Sheet Size
2. Select Alloy Type
3. Select Mesh Count

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Sheet
Net weight 0.0539 kg
Gross weight 0.0593 kg
Dimensions 18 x 18 x 0.025 cm
TDS, SDS & Technical Documents

Technical Specifications

Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
27–28 %

Additional Information

Alkaline Electrolyzer (1 Nm3/h) Test Data

Test Conditions

  • Electrode: Φ200 mm,  46 mesh (0.25 mm wire diameter) Raney Nickel
  • 24 units of electrolytic chambers
  • Applied current and voltage: 4700 mA/cm2 and 1.95 V
  • Temperature: 70 °C

Test Result

  • Power Consumption: 4.58 kWh/Nm3

Chemical Composition

Element Expected Concentration, Ni200 [wt%] Measured Concentration [wt%]
Nickel >99 99.36
Iron <0.4 0.21
Silicon <0.35 0.15
Copper <0.25 0.12
Sulfur <0.01 0.001
Manganese <0.35 0.16

Mechanical Properties

Property Value Unit
Elongation at Break 27–28 %
Tensile Strength 418 MPa

Leading Brands Trust in Our Products and Services